✉trading@fonhonmg.com ✆+86-13564036920 Magnesium Alloy Die Casting · Full-Process Manufacturing
FREE ENGINEERING TOOL

What is that defect telling you?

Pick the defect you can see on the casting. Each panel lists likely process causes and links to the engineering note that explains the mechanism. Use it to frame a question for your supplier — not as a substitute for a root-cause investigation.

Gas porosity

Round or irregular voids, usually found in thicker sections, near gates or after machining exposes the internal structure. In magnesium, gas porosity is strongly tied to melt protection and filling behaviour.

Likely process causes

  • Inadequate melt protection or excessive melt temperature
  • Entrapment from gate design or insufficient venting
  • Die temperature outside the process window
  • Vacuum system not holding during the shot
Ask for porosity by zone and by cavity, not a single pass/fail on one section.

Cold shut / cold lap

A visible line where two flow fronts met without fusing. Common on thin ribs, long flow paths and the last area to fill.

Likely process causes

  • Die too cold, or local cold zone in the cavity
  • Injection speed too low at the flow front
  • Melt temperature drop over a long flow length
  • Gate location making the front divide and rejoin
Raising the whole die temperature can make a hot spot worse. Look for a thermal map first.

Shrinkage porosity

Irregular, often interconnected voids in the last region to solidify. Unlike gas porosity, shrinkage is a feeding and solidification problem.

Likely process causes

  • Thick-to-thin transition without a gradual run-out
  • Gate or overflow placed where it cannot feed the boss
  • Local hot spot from cooling channel layout

Sticking / soldering

Metal adhering to the die face, visible as scuffing or build-up on cores and walls. It damages surface finish and eventually the die.

Likely process causes

  • Die temperature too high at the contact zone
  • Release spray amount or pattern inconsistent
  • Draft angle or surface finish of the die inadequate

Cracking

Cracks appearing at ejection, during trimming or later in service. The timing is as important as the appearance.

Likely process causes

  • Ejection while the part is still too hot or unevenly cooled
  • High-impurity zones raising internal galvanic attack
  • Stress concentrated at a sharp corner or machined interface

Flow marks

Surface patterns following the flow front. Often cosmetic, but they can indicate an unstable filling front that will cause deeper problems elsewhere.

Likely process causes

  • Speed changes along the flow path
  • Melt front cooling prematurely
  • Coating or die surface condition inconsistent