✉trading@fonhonmg.com ✆+86-13564036920 Magnesium Alloy Die Casting · Full-Process Manufacturing
FREE ENGINEERING TOOL

Magnesium vs aluminium: what does the part actually weigh?

Enter the material volume of your part and the annual quantity. The calculator compares magnesium AZ91D with aluminium ADC12 or steel, on part weight and material cost only. Tooling, machining, coating and freight are not included.

Your part

Default prices are indicative only. Edit them to your own contract terms. Volume is treated as solid equivalent material volume; draft allowances are not modelled.

Result

Material volume per part9.00 cm3
Magnesium part weight15.7 g
Comparison part weight24.3 g
Weight saving per part8.6 g (35.6%)
Weight saving per year86 kg
Material cost difference per yearUSD -1,765