Your Drawing Says "X-Ray per ASTM E505". Neither Standard Says What Fails.

Your Drawing Says "X-Ray per ASTM E505". Neither Standard Says What Fails.

Two standards, seventeen years and two languages apart, leave the reject line to the buyer. A 2026 revision project for GB/T 23600 makes this a good time to fix the drawing note.

A drawing note that says "X-ray per ASTM E505" looks like a quality requirement. It is not one yet. ASTM E505-22 is a set of reference radiographs: original film images showing categories and severity levels of discontinuities in aluminium and magnesium die castings. Its own Significance and Use says the pictures exist so that acceptance standards developed for particular requirements can be written in terms of them — in other words, it supplies the vocabulary, not the sentence. The standard's Scope calls them "example radiographic illustrations of discontinuities and a nomenclature for reference in acceptance standards, specifications, and drawings". A note that cites E505 and stops there requests an examination but gives the inspector nothing to reject against.

Seventeen years earlier and in another language, GB/T 23600-2009 made the same decision. Chapter 1 of China's X-ray real-time radioscopic testing method for magnesium alloy castings states plainly that the standard specifies the test method but "does not specify acceptance criteria for internal discontinuities in castings". Two standards, two standards bodies, same boundary. Both leave the pass/fail line to the drawing, the specification or the purchase order — which is exactly where most disputes begin.

Why one number for the whole part causes trouble

The E505 set is not a single scale. It contains five frames: the first four carry two sets each of four graded levels of increasing severity, and the last holds two ungraded images of foreign material. For magnesium there are three graded discontinuity categories, each at four levels, tied to specific section thicknesses — Category A at 1/8 in (3.2 mm) and 5/8 in (15.9 mm), Category B at 1/8 in, Category C at 5/8 in. A severity level quoted without a category and a thickness is not inspectable, because the reference plates are thickness-specific. E505's Note 2 points to ASTM E155 for thicker castings up to 2 in (50 mm). The 2022 edition also says film reference radiographs are not for direct comparison with digital images and directs digital work to ASTM E2973; E155 and E2422, used for other casting processes, grade in eight steps rather than four, so a level number copied from a sand-casting drawing does not carry over.

Then there is the geometry. Industry guidance on porosity disputes says the most common cause is a single severity level applied to an entire casting. It puts the tightest requirement on decorative surfaces where it buys nothing, and leaves the one sealing face or load-bearing web under-specified because nobody marked it as different. The usual remedy is zoning: a functional zone with the strictest level, a machined-skin zone, and an as-cast remainder that may have no radiographic requirement at all but still has to pass a leak test. Each zone needs a reference document, a discontinuity category, a maximum severity level, and a statement of what applies outside the zones. Both parties should hold the same reference image or an agreed physical section — E505 even asks users to check the films periodically for wear, since scratched reference plates change the comparison.

Related documents do not fill the gap. ASTM E94 and E1030/E1030M govern how the radiograph is produced and how good the image must be; E2698 covers digital detector arrays; none of them decides whether a part is acceptable. A general alloy specification will not do it either. A third-party testing page we found quotes porosity below 1.5% and a maximum single defect of 5% of wall thickness for cast magnesium wheels, but that is a laboratory's published service description, not a limit we would copy into a drawing without knowing the part and the customer's specification.

A revision is in progress

GB/T 23600-2009 was published on 15 April 2009 and implemented on 1 February 2010, refers to BS EN 13608.3-2001 in its foreword, and was reviewed on 1 July 2025 with a "continue in force" conclusion. On 28 April 2026 the standardisation administration assigned a revision project, plan number 20262447-T-610, under the National Technical Committee on Nonferrous Metals Standardisation; it is currently at the consultation stage, with a twelve-month cycle and a target completion in April 2027. The drafting group is led by Chongqing Boao Magnesium-Aluminium and includes Chongqing University, Shanghai Fangke, Ningbo Xingyuan Zhuomei, Wanfeng Meridian, an X-ray equipment maker, a testing and certification body and others. Related standards listed alongside it include GB/T 39638-2020 for digital radiography of castings, GB/T 25747-2022 for magnesium die castings and GB/T 13820-2018 for magnesium castings. We are not going to predict what the revised text will require; a consultation draft is not a published standard. But a method standard being revised while the acceptance criteria still sit outside it is a useful reminder of where the responsibility has always been.

What to put on the drawing instead

Name the examination practice, then zone the part: reference document, discontinuity category, maximum severity level and the nearest illustrated thickness for each zone; a statement about areas outside the zones; whether digital imaging is permitted and against which digital reference set; the leak test or machined-face criterion where porosity matters functionally; and the sampling plan and record retention in the purchase order. Ask the supplier a commercial question alongside it: what does that level require in tooling, vacuum assistance and cycle time on this part? Some levels are reachable with disciplined venting on a standard HPDC cell; others need vacuum, squeeze or semi-solid routes. A buyer who quotes the tightest level while paying for the first group has created a quotation that cannot be built.

We keep tooling, die casting, precision machining and surface treatment in one plant in Ningbo, so we can discuss the zone map and the process needed to hold it before steel is cut. That does not make us the authority on a customer's acceptance standard — the limit is theirs to write — and we would rather say so. Send the drawing with the zones marked, or see the process scope. For why a trial result is not a production rate, see the yield-to-SOP note; for how a number in a quotation changes with its assumptions, the die-life note; and for the paperwork that travels with an export order, the 2026 customs decision.

The short version

E505 shows what a defect looks like; GB/T 23600 describes how to see it. Neither says how much is too much. If your drawing does not say, the argument starts at first article inspection instead of at quotation.

Frequently Asked Questions

Does ASTM E505 tell us what level of X-ray defect fails a casting?

No. ASTM E505-22 is a set of reference radiographs: it supplies the vocabulary for writing acceptance standards, not the sentence itself. The article notes that a note citing E505 and stopping there requests an examination but gives the inspector nothing to reject against.

What does GB/T 23600-2009 say about acceptance criteria?

Chapter 1 states plainly that the standard specifies the test method but does not specify acceptance criteria for internal discontinuities in castings. Two standards, seventeen years and two languages apart, leave the reject line to the buyer.

Why is a single severity level for the whole part a problem?

Because the reference plates are thickness-specific. A level quoted without a discontinuity category and a thickness is not inspectable, and the common outcome is that decorative surfaces get the tightest requirement while the sealing face or load-bearing web is left under-specified.

What is the fix on the drawing?

Zone the part. Each zone needs a reference document, a discontinuity category, a maximum severity level, the nearest illustrated thickness, and a statement of what applies outside the zones. Both parties should hold the same reference image or an agreed physical section.

Can a level number be copied from a sand casting drawing?

No. ASTM E155 and E2422, used for other casting processes, grade in eight steps rather than four, so a level copied from another process does not carry over. The 2022 edition also states that film reference radiographs are not for direct comparison with digital images.

Is the Chinese standard being revised?

Yes. A revision project, number 20262447-T-610, was assigned on 28 April 2026, is currently at consultation stage, with a twelve-month cycle and target completion in April 2027. The article does not predict what the revised text will require.

What commercial question should accompany the acceptance level?

What that level requires in tooling, vacuum assistance and cycle time on this part. Some levels are reachable with disciplined venting on a standard HPDC cell; others need vacuum, squeeze or semi-solid routes. A buyer quoting the tightest level while paying for the first group creates a quotation that cannot be built.

Need magnesium alloy parts for your project?

Get a Quote →