Magnesium Prices Turn Up Again: Who Carries the Cost on a Quoted Order?

A November 27 US-date quotation puts Shaanxi Mg99.90 at RMB 15,750 per tonne, up RMB 250 on the week. The direction matters more than the number — especially for orders already priced.
A November 27, 2026 market note reports that magnesium and aluminium prices turned higher in the final week of the month. According to the Magnesium Branch of the China Nonferrous Metals Industry Association, the weighted average price of Mg99.90 primary magnesium in Shaanxi reached RMB 15,750 per tonne, up RMB 250 over the week. Producing regions in Shanxi and Ningxia also rose, and aluminium reversed after a run of declines.
For a buyer, the temptation is to translate RMB 250 into a new casting price. That is too simple. The figure is a weekly weighted average for primary magnesium in one province. It is not the increase paid for every alloy, and it is not a forecast. What matters is the change in direction after months of falling prices, and what that does to an order already quoted.
Why direction matters more than the weekly number
When metal is falling, a buyer can wait and expect the next quote to be no worse. When it turns, the cost basis for material bought afterwards changes. A die caster holding low-priced inventory may not raise a price immediately; a die caster replenishing now will. The effect appears gradually as old stock is consumed and replacement purchases are made, not uniformly across all work at once.
The same note is careful about aluminium: the reversal is reported, but the size of the increase is not established from the available information. A programme using both metals cannot assume the two moved by the same amount. Our total-cost framework puts metal, forming, finishing and service life in separate columns for exactly this reason.
Who carries the cost on an order already priced
This is a contract question. Where the selling price is fixed and replacement material costs more, the supplier's margin on that work is compressed. Where the pricing terms allow material costs to be reviewed, the effect is shared differently. The market report does not say which arrangement any individual caster uses, so a buyer should not guess — ask.
A workable clause states the index, the base month, the review frequency and the band inside which nothing changes. It should also say which alloy grade the index applies to and when the new price takes effect. Without those details, "price subject to material changes" is a phrase, not a clause. We have written about ingot price versus casting price and about the supply side behind the low price.
Expectation is not the same as a production cut
The reported driver of the rebound is expectation of production cuts and supply-demand adjustment. An expectation is not a confirmed reduction in output. Whether the rise lasts depends on what happens to actual supply and demand after the week. A short-lived move and a sustained increase create different purchasing pressure, even when both raise the price of an immediate order.
This distinction matters when a supplier warns that "prices are going up". Ask what has actually happened to output, which regions are affected, and whether the change has been confirmed by more than one source. The November quotation is a reference point for that week, not a forecast for the next quarter.
The rebound is not confined to one region
Rises in Shaanxi, Shanxi and Ningxia show the move was broader than a single local quotation. They do not show that all regions rose by the same amount, or that prices will keep rising. Buyers should treat the regional spread as a reason to name the producing region in the purchase order, not as a reason to chase the market.
Chasing is usually the wrong response. Earlier this month, similar production-cut expectations lifted prices and then faded. A buyer who changes suppliers on a one-week move pays for the transition twice.
The two-metal problem
Many programmes use both alloys: a magnesium housing with aluminium brackets, or an aluminium structure with magnesium covers. When both markets turn at once, a clause tied to a single index misses half the cost. Ask for two base dates and two review rules, and state which part carries which metal.
The direction of the two moves may also differ. The note reports an aluminium reversal without quantifying it, so a buyer cannot assume the same percentage applies. A supplier who quotes a single "material adjustment" for a mixed assembly is simplifying a real problem — usually in the supplier's favour.
What to put in the next RFQ
Four lines are enough: the alloy grade and producing region, the price base date, the index and review band, and the lead time for a price change to take effect. Add a line for aluminium if the same programme uses both metals. Then ask the supplier how much material is already purchased for your order — a question that tells you more about the next quote than the weekly headline.
Where to start
We state the assumptions behind a quotation and keep tooling, casting, machining and finishing in one plant in Ningbo. Send the part, the volume and the target price base and we will tell you which term needs to be written down first.