Your Part Was In Tolerance. Then It Grew on the Way to the Customer.

Your Part Was In Tolerance. Then It Grew on the Way to the Customer.

Magnesium expands at roughly twice the rate of steel, and a casting cools from a 200 °C die. Where the numbers move, and how to write a drawing that survives the trip.

A magnesium part can leave your plant inside every tolerance on the drawing and arrive outside them. The reason is arithmetic. AZ91D's linear thermal expansion is around 25 to 27 µm per metre per kelvin, against about 22 to 23 for the aluminium it replaced and 11 to 14 for the steel bearings, shafts and bolts it gets bolted to. One material data sheet puts it plainly: a 100 mm part grows 125 µm over a 50 °C rise. Another note on magnesium motor housings puts the same comparison in context, adding that the ceramic layer of a micro-arc oxidation coating expands at only 5 to 10 µm per metre per kelvin, so the metal underneath moves three to five times more than the coating sitting on it.

Magnesium also leaves the die hot. A casting cools from a die at 200 to 300 °C, and if that cooling is not even, the part warps and carries residual stress into machining. And because magnesium alloys cannot be heat-strengthened the way aluminium can be given a T6 treatment, there is no later thermal step available to pull the dimensions back. What you have at the end of the process line is what the process gave you.

Where the measurement goes wrong

The most common defect report on a magnesium part is not a bad casting. It is a part that was measured too early, or too warm, or in the wrong place. A published process note on magnesium machining makes the point directly: a common error that compromises CMM accuracy is measuring a part that has not fully cooled after machining, because a warm part gives false readings and the component is out of tolerance once it reaches ambient temperature. The same note lists the three elements it calls non-negotiable for precision work — a temperature-controlled workshop, temperature-controlled coolant, and a workpiece at a stable temperature — with adequate stabilisation time before final inspection treated as a quality gate.

Precision requirements go further still. One aerospace-grade machining write-up describes its metrology regime: continuous climate control at 20 °C ±0.5 °C, thermal stabilisation soak periods of 24 hours, and coordinate measuring machines with a maximum permissible error of 0.9 + L/350 µm. It also shows what a disciplined magnesium program looks like in practice — rough machining leaving 0.35 mm per side, an intermediate thermal cycle at 200 °C for two hours between operations, then finish machining with PCD tooling at a cutting speed of 1,100 m/min, producing a bore concentricity of 0.006 mm and flange flatness of 0.004 mm on the first article.

What temperature does after the machining

The last point is the one most drawings forget. A coating operation is a second heat treatment. A powder or e-coat cure at 150 to 200 °C will move the part, and whether it moves inside tolerance depends on how much residual stress the casting carried and where the part was clamped. Heat-soaking a housing before pressing in a bearing is a thermal shock event with a coefficient mismatch at every interface. And in service, a magnesium housing at operating temperature grows against a steel bearing and a steel shaft at roughly twice the rate: bearing preload changes, the rotor-stator air gap changes, and the clamping force of bolted joints drops. These are consequences of one material property, and they arrive whether or not the drawing mentions it.

How to write it so the part survives the trip

Three things belong on the drawing and in the inspection report. First, the temperature at which the dimensions apply, stated as 20 °C unless the customer says otherwise, and a note that the drawing tolerances are valid at that temperature. Second, the stabilisation requirement: how long the part must sit before measurement, and whether the measurement is taken on the part as-machined or after a stress-relief cycle. Third, a statement about which surfaces are critical, because the thermal story is not uniform across a casting: a machined bearing seat and a cast web do not move by the same amount, and the drawing should say which one the tolerance is about.

On the commercial side, the question worth asking a supplier is not "is your tolerance capable". It is "at what temperature, after how long, and measured how". Two suppliers quoting the same tolerance on paper can be describing two different inspections, and the difference shows up as a rejection at your customer's dock rather than at your CMM.

We keep tooling, die casting, precision machining and surface treatment in one plant in Ningbo, so the sequence from casting through machining to coating happens under one roof and one set of shop conditions — which is what makes the dimensional story at least consistent internally. It does not make it temperature-proof at your site, and we would rather say so. Send the drawing and the temperature it will be measured at, or see the process scope. For the housing that has to survive heat as well as load, see our note on e-drive housings; for what a number in a quotation assumes, see our note on die life and amortisation.

The one-line version

A tolerance without a temperature is not a tolerance. It is a number that waits for the truck to deliver the weather.

Frequently Asked Questions

How much does a magnesium part grow between the factory and the customer?

AZ91D's linear thermal expansion is around 25 to 27 µm per metre per kelvin, against about 22 to 23 for aluminium and 11 to 14 for the steel bearings, shafts and bolts it gets bolted to. A 100 mm part grows 125 µm over a 50 °C rise.

Does a coating move the part too?

Yes. A note on magnesium motor housings puts the ceramic layer of a micro-arc oxidation coating at only 5 to 10 µm per metre per kelvin, so the metal underneath moves three to five times more than the coating sitting on it.

Why can a part measure in tolerance and still be out of tolerance later?

Because it was measured too early or too warm. A published process note states that measuring a part that has not fully cooled after machining gives false readings and the component is out of tolerance once it reaches ambient temperature.

What does a high-precision magnesium program look like?

One aerospace-grade write-up describes continuous climate control at 20 °C ±0.5 °C, thermal stabilisation soak periods of 24 hours, and CMMs with a maximum permissible error of 0.9 + L/350 µm, with a 200 °C two-hour stress-relief cycle between operations.

What three things belong on the drawing?

The temperature at which the dimensions apply, stated as 20 °C unless the customer says otherwise, the stabilisation requirement before measurement and whether it is measured as-machined or after stress relief, and which surfaces are critical, since a machined bearing seat and a cast web do not move by the same amount.

What should a buyer ask a supplier instead of asking can you hold the tolerance?

At what temperature, after how long, and measured how. Two suppliers quoting the same tolerance on paper can be describing two different inspections, and the difference shows up as a rejection at your customer's dock rather than at your CMM.